Skup podataka: izc_experimental_data.zip, 37.08 MB Pravo pristupa: Otvoren pristup Opis datoteke: Experimental data containing PXRD, SEM, TEM, SS-NMR, Raman and LLS datasets (engleski)
Prijavite se u repozitorij kako biste mogli spremiti objekt u svoju listu.
Citirajte ovaj rad
Jakupec, N. (2024). Experimental data for paper titled "Mechanochemically induced OSDA-free interzeolite conversion" [Skup podataka]. https://urn.nsk.hr/urn:nbn:hr:241:703267.
Jakupec, Nikola. Experimental data for paper titled "Mechanochemically induced OSDA-free interzeolite conversion". Institut Ruđer Bošković, 2024. 27.12.2024. https://urn.nsk.hr/urn:nbn:hr:241:703267.
Jakupec, Nikola. 2024. Experimental data for paper titled "Mechanochemically induced OSDA-free interzeolite conversion". Institut Ruđer Bošković. https://urn.nsk.hr/urn:nbn:hr:241:703267.
Jakupec, N. 2024. Experimental data for paper titled "Mechanochemically induced OSDA-free interzeolite conversion". Institut Ruđer Bošković. [Online]. [Citirano 27.12.2024.]. Preuzeto s: https://urn.nsk.hr/urn:nbn:hr:241:703267.
Jakupec N. Experimental data for paper titled "Mechanochemically induced OSDA-free interzeolite conversion". [Internet]. Institut Ruđer Bošković: Zagreb, Ruđer Bošković Insistute, Bijenička Cesta 54, HR; 2024, [pristupljeno 27.12.2024.] Dostupno na: https://urn.nsk.hr/urn:nbn:hr:241:703267.
N. Jakupec, Experimental data for paper titled "Mechanochemically induced OSDA-free interzeolite conversion", Institut Ruđer Bošković, 2024. Citirano: 27.12.2024. Dostupno na: https://urn.nsk.hr/urn:nbn:hr:241:703267.
PXRD patterns were collected using PANalytical Aeris benchtop powder diffractometer (CuKα radiation with Ni filter; λ= 1.5418 Å, 45 kV, 40 mA) in Bragg-Brentano geometry in a 5°-50° 2θ range (0.025° step).
Particle size distribution (PSD) curves were obtained by laser light scattering analysis using Malvern Mastersizer 2000 laser light scattering granulometry. The samples were exposed to ultrasonication during the measurement.
Scanning electron microscopy (SEM) images were acquired on a Jeol JSM 7000F scanning electron microscope and a MIRA-LMH (TESCAN) scanning electron microscope equipped with a field emission gun.
Solid-state nuclear magnetic resonance spectroscopy measurements were performed on a 600 MHz Varian spectrometer, using 3.2 mm HX CPMAS probe to obtain 27Al MAS, 29Si MAS and 1H-29Si CPMAS spectra. All of the samples were measured under magic-angle spinning frequency of 20 kHz. Operating Larmor frequencies for 1H, 27Al, and 29Si nuclei were 599.34 MHz, 156.17 MHz and 119.06 MHz, respectively. To obtain directly detected 27Al and 29Si MAS spectra a single pulse of 1.0 µs with recycle delay of 0.1 s and a single pulse of 2.8 µs with recycle delay of 60 s was used, respectively. In the case of 1H-29Si CPMAS measurements, a single pulse of 2.85 µs was used to excite 1H nuclei with a following contact time of 5.0 ms to transfer the polarization to 29Si nuclei, recycle delay was 1.0 s. NMR spectra were deconvoluted using dmfit software.
Transmission electron microscopy (TEM) analysis was carried out on a FEI Talos F200X microscope operated at 200 kV. The samples were measured with high-resolution TEM (HRTEM), fast Fourier transform (FFT), and electron diffraction (ED) techniques.
Chemical composition of selected samples was assessed on the grounds of results obtained by a PerkinElmer AAnalyst 200 atomic absorption spectrometer.
The N2 physisorption isotherms were measured at −196 °C utilizing Micromeritics 3Flex high resolution volumetric adsorption analyser. About 100 mg of the sample was degassed at 300 °C under vacuum overnight prior to the analysis. Micropore volume (Vmic) was evaluated on the grounds of the t-plot method, and total pore volume (Vtot) was determined by the amount of adsorbed nitrogen at p/p0 = 0.95. Mesopore volume (Vmeso) is defined as Vtot - Vmic.
Raman spectra of the powder samples were collected employing Maya2000 Pro spectrometer in Raman spectroscopy mode using red laser (785 nm). The interval time for each scan was set to 5000 ms, and the number of scans per interval was 80 at a laser power of 60 mW. Each sample was put on a thin glass slice and levelled with a spatula to ensure surface flatness.
Zagreb, Ruđer Bošković Insistute, Bijenička Cesta 54, Hrvatska
Geolokacija
Hamburg, DESY, Notkestraße 85, Njemačka
Geolokacija
Berlin, Institute of Physics, Humboldt University of Berlin, Newtonsraße 15, Njemačka
Geolokacija
Ljubljana, National Institute of Chemistry, Hajdrihova ulica 19, Slovenija
Projekt
Šifra: UIP-2019-04-4977 Naziv (hrvatski): Zeoliti s malim šupljinama modificirani bakrom pogodni za primjenu u zaštiti okoliša Naziv (engleski): Copper-modified Small-pore Zeolites Suitable for Environmental Applications Kratica: SMALLPORE Voditelj: Ana Palčić Pravna nadležnost: Hrvatska Financijer: HRZZ Linija financiranja: UIP